Steel Grade Equivalents: EN, ASTM, JIS and GB

Nov 12, 2026

Leave a message

Lissandra
Lissandra
Export sales at Kennen Steel International. Works with overseas buyers on steel plate, coil and pipe sourcing from vetted Chinese mills.

EN 10210 S355J2H hot finished hollow sections

"Equivalent grade" is one of the most dangerous phrases in steel procurement. Two grades can have the same yield strength, the same carbon range and still not be substitutable, because one requires impact testing and the other does not, or one is killed and fine-grained while the other is not.

Here is a working comparison, and the places where you should not treat the numbers as permission.

The common pairs

EN ASTM JIS GB Notes
S235JR A283 Gr.C SS400 (approx.) Q235B Yield match, impact differs
S355JR A572 Gr.50 (approx.) SM490A Q345B A572 has no mandatory impact test
S355J2 A572 Gr.50 + Charpy SM490B Q345D J2 needs −20 °C impact; A572 base spec does not
S275JR A36 SS400 Q275 A36 has a tensile range, not a yield minimum in the same way
P265GH A516 Gr.60 - Q245R Pressure vessel, different design allowables
P355NH A516 Gr.70 - Q345R Same warning
304 S30400 SUS304 06Cr19Ni10 Practical equivalence
316L S31603 SUS316L 022Cr17Ni12Mo2 Practical equivalence

Where equivalence breaks

Impact testing. S355J2 and A572 Gr.50 are routinely treated as interchangeable. They are not, unless the A572 is ordered with supplementary Charpy testing at the required temperature. A designer specifying S355J2 has chosen a low-temperature material; A572 without impact data does not deliver that.

Pressure vessel grades. P265GH and A516 Gr.60 both work at elevated temperature, but the allowable stress tables, the permitted chemistry ranges and the testing requirements differ between EN 13445 and ASME VIII. A substitution changes the design calculation, and that is an engineering decision, not a purchasing one.

Killed vs rimmed steel. Older GB grades were available in rimmed (沸腾钢) form; S235JR is always killed. For anything welded or dynamically loaded, only killed, fine-grained steel should be accepted, regardless of what the strength table says.

Delivery condition. "S355J2" says nothing about whether it is as-rolled, normalized or TMCP. The same grade in different conditions has different toughness and different weld behaviour. Always specify +N or +AR.

How to use a comparison table properly

  1. Compare the full requirement set, not just yield. Strength, impact, chemistry, delivery condition, testing and certification.
  2. Write the substitution into the contract if you accept one, with the supporting test requirements. Verbal agreement on "equivalent" is worthless at the inspection stage.
  3. Ask for both certificates if you are substituting - the original and the proposed - and have your engineer confirm the design still works.
  4. Do not substitute on pressure or lifting equipment without written design approval.

How we supply against mixed standards

Buyers frequently have a European drawing, a Chinese fabricator and an ASTM-based inspector on the same job. That is exactly where substitutions go wrong, so we handle it explicitly:

  • We read the specification clause, not just the grade name, and quote the grade plus the delivery condition and testing that satisfy it
  • Where a Chinese GB grade is genuinely equivalent, we say so and provide the comparison basis; where it is close but not equal, we say that too
  • Certificates are issued to the standard in the contract - if your contract says EN 10025-2, we do not ship a GB/T certificate with an EN translation
  • For projects with multiple standards, we can supply a single consolidated comparison sheet for your engineer to sign off before production

Send us the drawing and the standard list. We will come back with the actual grades we can offer, what testing they carry, and where the gaps are.

Related products: Hot rolled products, Structural steel sections, Fasteners

Frequently asked questions

Is S355J2 the same as A572 Gr.50?

Only if the A572 is ordered with supplementary Charpy testing at minus 20 C. The base A572 specification does not require impact testing.

Can Q235B replace S235JR?

They are close on strength and both are killed steels, but the certification and testing requirements differ. Confirm the substitution in writing.

Are pressure vessel grades interchangeable?

No. Allowable stress tables and testing requirements differ between EN 13445 and ASME VIII, so a substitution is an engineering decision.