The three S355 grades have almost the same chemistry and the same 355 MPa minimum yield. What separates them is one thing: the temperature at which the Charpy impact test is carried out. JR is tested at +20 °C, J0 at 0 °C and J2 at −20 °C, all with a 27 J minimum average.
The price difference is usually 3–5%. The cost of getting the grade wrong is not 5% - it is rejected material on site, a stalled project, or a brittle failure in winter. So the question is not "which grade is better" but "how cold can this structure get?"
The three grades side by side
| Grade | Impact test temp | Min. average energy | Typical use |
|---|---|---|---|
| S355JR | +20 °C | 27 J | Indoor structures, warm climates, general fabrication |
| S355J0 | 0 °C | 27 J | Outdoor structures in temperate climates, CE-marked work |
| S355J2 | −20 °C | 27 J | Cold climates, offshore, crane booms, dynamic loads |
| S355J2+N | −20 °C | 27 J | Same as J2, supplied normalized (+N) |
All three share the same tensile range (470–630 MPa) and the same chemistry limits. J2 and J0 also carry a sub-grade letter for the energy level at the lower test temperature (JR/J0 = 27 J only; J2 has K2 = 40 J option).
How to pick in practice
Start from the lowest temperature the steel will see in service, not the temperature at the port.
- Indoor, heated, or tropical sites - JR is enough and it is the cheapest.
- Outdoor structures in Europe, Turkey, North Africa - J0 covers most cases, but check the project specification. Many EN-based designs default to J2 regardless of climate, because the designer does not want to argue about it later.
- Anything north of the Alps, in Canada, Central Asia, or with impact loading - J2. A crane boom in Rotterdam still needs J2 because the design code says so.
- Pressure vessels and boilers - a different family entirely (P355NH / A516). Do not substitute S355J2 here.
There is also a thickness effect that catches people: impact energy drops as plate gets thicker, and above roughly 40 mm the mill may need a different rolling and heat treatment route (normalized, or TMCP) to hold the values. A 60 mm S355J2 plate is not the same product as a 10 mm one.
Three things buyers get wrong
- Reading "S355J2" on the mill certificate and stopping there. The certificate has to show the test temperature and the individual impact values. If the values are at +20 °C, you have JR with a J2 label.
- Assuming CEV is included. For S355, the carbon equivalent matters for weldability, and the limit differs by thickness (0.45 for ≤ 30 mm, 0.47 above). Ask for CEV on the certificate if you are welding heavily.
- Mixing grades in one bundle. If one heat is J2 and the next is JR, the packing list must separate them. Colour coding at the mill helps, but only your own incoming inspection really settles it.
How we supply S355
We source S355JR, J0 and J2/N from Chinese mills that roll to EN 10025-2 with the impact test done at the required temperature, not at ambient and then relabelled. Concretely:
- Thickness 6–150 mm, widths up to 3,000 mm, cut to your sizes or supplied as full plates
- EN 10204 3.1 certificate per heat, with test temperature and individual Charpy values shown
- CEV reported on request; UT (ultrasonic) testing to EN 10160 on request
- Third-party inspection (SGS, BV, Intertek) arranged before shipment if your project requires it
- Edge preparation, drilling and primer coating available through our processing partners
If you are unsure which grade your design actually calls for, send us the drawing or the specification clause. We will tell you what it translates to in EN/ASTM terms and quote the grade that meets it, not the one that is easiest to ship.
Related products: S355J2+N steel plate, S355J0 steel plate, S235JR steel plate
Related reading
Frequently asked questions
Can S355J2 be used instead of S355JR?
For most structural work yes, at 3 to 5 percent higher cost. The reverse is not true: S355JR cannot substitute for S355J2 where impact testing at minus 20 C is specified.
What test temperature does S355J2 require?
Charpy V-notch impact testing at minus 20 C, with a 27 J minimum average on three specimens.
Is S355JR suitable for outdoor use in winter?
Only if the design temperature stays above 0 C. Below that, specify S355J0 or S355J2 and ask for the impact values on the certificate.