Wear Plate Selection: NM400, NM450 or NM500
Wear plate is bought by hardness number and used by application. The three common grades differ by about 100 HBW each, and the price difference is smaller than the cost of replacing the wrong one.
The grades in practice
| Grade | Hardness (HBW) | Typical use | Relative cost |
|---|---|---|---|
| NM400 / AR400 | 360–440 | Truck bodies, buckets, chute liners, general wear | Base |
| NM450 / AR450 | 420–480 | Mining truck beds, crusher liners, heavy abrasion | +8–15% |
| NM500 / AR500 | 470–540 | High impact plus abrasion, screen decks, cutting edges | +15–25% |
Hardness is not the only variable. Toughness decides whether the plate cracks when a rock hits it, and toughness falls as hardness rises. On a primary crusher feed chute, NM500 can crack where NM450 would dent - and a dented liner can be straightened, a cracked one cannot.
How to choose
- Fine abrasion, low impact (conveyor skirts, hoppers): NM400 is usually enough
- Mixed abrasion and impact (truck beds, loader buckets): NM450 is the usual compromise
- High impact at a point (crusher jaw area, cutting edges): NM500, but check the welding procedure
- Hot abrasion (above about 250 °C): wear plate hardness drops, and a different material class may be needed
Fabrication cautions
Wear plate is quenched and tempered, so the heat input during welding matters:
- Use low hydrogen consumables and controlled interpass temperature
- Avoid welding near the plate edge without pre-heat; edge cracking starts there
- Do not flame cut and then weld the same edge without removing the hardened zone
- Bolt where possible - a bolted liner is replaceable, a welded one is a repair
Buying checks
Ask for surface hardness measured on the delivered plate, not the mill's nominal. Delivered hardness is typically tested at several points and can vary by 20–30 HBW across a plate. Also confirm the thickness: wear plate is often supplied to a minimum thickness, and 20 mm nominal may arrive at 19.2 mm.
How we supply
- NM400, NM450 and NM500 from mills rolling to GB/T 24186 or equivalent, with hardness tested and reported
- Thickness 6 to 100 mm, cut to size or profiled to your drawing
- EN 10204 3.1 certificate including hardness values per plate
- Cutting and edge preparation through our processing partners, with the hardened zone removed where welding is specified
Send the application, the abrasive and the impact conditions. We will recommend the grade, and tell you when the cheaper one is the better engineering choice.
Related: Hot rolled plate, Wear resistant plate, Dimensional checks on arrival
Frequently asked questions
Is NM500 always better than NM400?
No. Higher hardness means lower toughness, so NM500 can crack under impact where NM450 would dent.
Can wear plate be welded normally?
It needs low hydrogen consumables and controlled heat input, and flame-cut edges must be cleaned before welding.
Should hardness be tested on delivery?
Yes. Delivered hardness can vary by 20 to 30 HBW across a plate, so test rather than assume the nominal value.