Both are zinc-based coatings on steel coil, both are sold by coating weight, and both are used for roofing, cladding and light structures. The difference is the alloy, and it decides how the material behaves in your climate.
What the numbers mean
Z275 means 275 g/m² of zinc coating (both sides combined), which is roughly 20 µm per side. AZ150 means 150 g/m² of a 55% aluminium / 43.4% zinc / 1.6% silicon alloy coating, roughly 20 µm per side as well.
So the coating weights are close but the materials are not. Zinc protects steel sacrificially: it corrodes first and protects cut edges. Aluzinc is more barrier than sacrificial - the aluminium-rich layer resists long-term atmospheric attack better, and it holds up at higher temperatures, but it protects exposed cut edges less well than pure zinc.
Where each one wins
| Z275 galvanized | AZ150 aluzinc | |
|---|---|---|
| Corrosion in rural / urban atmosphere | Good | Better, typically 1.5–2× the life of Z275 at equal coating mass |
| Cut edge protection | Strong | Weaker, edges need attention |
| Heat resistance | Degrades above ~200 °C | Good to around 300 °C, better for chimney and oven parts |
| Appearance | Matte grey, spangles visible | Smooth, lighter, more uniform; paints well |
| Welding | Easier | More difficult, coating can fume |
| Alkaline contact (fresh concrete, wet cement) | Better | Poor - aluzinc dislikes alkaline environments |
| Typical use | General roofing, ducting, framing, agriculture | Roofing and cladding in harsh atmospheres, appliances, ovens |
How to decide
Look at the environment and the fabrication, not the price list.
- Coastal, industrial or high-humidity sites - AZ150 usually gives longer life for the same weight.
- Cut edges exposed and the part is heavily sheared - Z275 is safer; the zinc keeps protecting the exposed edge.
- In contact with concrete, mortar or animal waste - plain galvanized. Aluzinc is not the right choice in alkaline conditions.
- Painted product where appearance matters - AZ150 takes paint well and gives a smoother base, but the pre-treatment has to be correct.
- Anything above 200 °C in service - aluzinc, unless you go to stainless.
One more thing worth saying out loud: coating mass is not the only variable. The substrate matters just as much. An AZ150 on a DX51D substrate is a different product from AZ150 on S250GD or S350GD structural grade. Buyers who compare only coating weight often miss that.
How we supply coated coil and sheet
- Hot dip galvanized coil, Z120–Z275, in DX51D, S250GD, S280GD and S350GD
- Aluzinc coil, AZ100–AZ150, in DX51D and structural grades
- Widths 600–1,250 mm, thickness 0.2–2.0 mm, coil or cut sheet
- Chromate-free passivation, anti-finger print, or oiled, per your downstream process
- Slitting to your widths, with edge condition agreed in writing
- EN 10204 3.1 certificate plus coating mass test results from the line
If you are choosing between the two for a specific site, tell us the location, the exposure and the expected service life. We will recommend a coating and a substrate together, because quoting one without the other is how people end up with a coil that rusts in two years.
Related products: AZ150 aluzinc coil, Galvanized coil
Related reading
Frequently asked questions
Is AZ150 better than Z275?
It lasts longer in most atmospheres at equal coating mass, but it protects cut edges less well than pure zinc.
Which coating should I use near the coast?
AZ150 usually gives 1.5 to 2 times the service life of Z275 at the same coating weight.
Can aluzinc be used in contact with concrete?
No. Alkaline contact attacks the aluminium-zinc coating. Use galvanized for concrete, mortar or animal waste exposure.